Self-lubricating bearings the main fault note

Since smooth bearings in the job because the journal and bearing touch a conflict occurs, resulting in the appearance of heat, wear, even “killed” and other problems, so when depicted bearing, should be used with good anti-friction bearing bush materials production, appropriate Glazes and choose the appropriate supply of ways to improve the layout in order to obtain a thick film bearing smooth and so on.
1, tile surface corrosion: spectral analysis found abnormal concentrations of non-ferrous metal element; bearing presents submicron wear particles of many non-ferrous metal components; lubricating oil moisture overruns, Koh overruns.
2, the outer corrosion journal: spectral analysis found abnormal concentrations of iron, bearing in many submicron particles of iron component, moisture overruns or lubricating oil acid value overruns.
3, tile shedding: bearings were found to have many large-scale fatigue shedding alloy wear particles, layered abrasive grains.
4, tile back fretting: spectral analysis found abnormal concentrations of iron, iron-bearing components in many sub-micron wear particles, water and an acid number of abnormal smooth oil.
5, since the smooth outer bearing strain: bearings were found to have cutting abrasive, abrasive component of non-ferrous metals.
6, the composite outer strain journal: Bearing in the presence of an iron-based cutting temper color or black oxide abrasive particles, metal appearance.
7, the bearing bush-burning: bearing alloy grains have more large-scale black and metal oxides.

dubushings

Our company is a professional manufacturer on various kind of bearings in China for over 15 years.If you are interested in our company's bearing and want to get the relevant information. You can consult our number: 0086-731 84770165, Email:bushings@slide-bearing.com or left click on the website customer service online consultation.

You may also like...

Leave a Reply

Your email address will not be published. Required fields are marked *